Steels. Determination and verification of the depth of carburized and hardened cases

Steels. Determination and verification of the depth of carburized and hardened cases

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1   Scope

This International Standard defines the case-hardened depth, and specifies methods for the determination of this depth, in steel.
It is applicable to
  1. a) carburized cases and carbonitrided cases;
  2. b) parts that, when heat treated to final hardness, have a hardness of less than 450 HV 1 at a distance of three times the case-hardened depth, from the surface.
The case-hardened depth is defined by special agreement where these conditions are not met.
For steels that, in the part under test, and at a distance of three times the case-hardened depth from the surface, present a hardness greater than 450 HV 1, the criterion can still be used, provided that a limiting hardness value greater than 550 HV 1 – in steps of 25 units – be selected for the case-hardened depth.