1. Scope*
1.1 This test method covers determination of transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry.
NOTE 1— True heats of fusion are to be determined in conjunction with structure investigation, and frequently, specialized crystallization techniques are needed.