Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry

Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry

Regular price
£68.00
Sale price
£68.00
Regular price
£61.20
Sold out
Unit price
per 

1.   Scope*

This test method outlines a procedure for the determination of oxidative-induction time (OIT) of polymeric materials by differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized/compounded form.