Specification and qualification of welding procedures for metallic materials. Welding procedure specification - Laser beam welding

Specification and qualification of welding procedures for metallic materials. Welding procedure specification - Laser beam welding

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

BS EN ISO 15609-4:2009 Specification and qualification of welding procedures for metallic materials. Welding procedure specification. Laser beam welding

BS EN ISO 15609-4 specifies requirements for the content of the welding procedure specification (WPS) for laser beam welding processes, including overlay welding. It does not apply to other processes for cladding (e.g. thermal spraying).

BS EN ISO 15609-4 is part of a series of standards, and details of this series are given in ISO 15607:2003, Annex A.

BS EN ISO 15609-4 lists variables that influence the quality and properties of the welded joint.

The dimensions mentioned in BS EN ISO 15609-4 influence the metallurgical and mechanical qualities, the geometry of the structural member and other important performance properties.

Contents of BS EN ISO 15609-4:

  • Foreword
  • Scope
  • Normative references
  • Terms and definitions
  • Technical content of welding procedure specification
  • General
  • Welding process
  • Manufacturer
  • Equipment
  • Parent materials
  • Filler or other additional material(s)
  • Joint design
  • Joint and surface preparation
  • Jigs, fixtures and tooling
  • Welding position
  • Backing Welding technique
  • Welding
  • parameters
  • Preheating and post-weld heat treatment
  • Operations after welding
  • Examples of welding procedure specification