1 Scope
This standard specifies test conditions and the procedure to be followed for determining
the tear strength of a trapezoidal specimen of a rubber- or plastics-coated fabric, using
a tensile testing machine. This test may be carried out:
-
— either on test specimens conditioned in reference atmospheres; or
-
— on test specimens which have been subjected to any necessary treatment for the application considered, for example dipping.