Resistance welding. Procedure for the evaluation of the life of spot welding electrodes using constant machine settings

Resistance welding. Procedure for the evaluation of the life of spot welding electrodes using constant machine settings

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

BS EN ISO 8166:2003 specifies a laboratory test procedure for the determination of the acceptable welding current range and the assessment of electrode life using a multi-spot test with specific conditions. This document is applicable for the assessment of the weldability of uncoated and coated sheet steels of thicknesses up to 3 mm. The test procedure specified in this document and the results obtained, apply only for the introduction of a new type or batch of material.