Plastics. Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics
Plastics. Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics
  • Load image into Gallery viewer, Plastics. Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics
  • Load image into Gallery viewer, Plastics. Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics

Plastics. Differential scanning calorimetry (DSC) - Part 7: Determination of crystallization kinetics

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1   Scope

This part of ISO 11357 specifies two methods (isothermal and non‑isothermal) for studying the crystallization kinetics of partially crystalline polymers using differential scanning calorimetry (DSC).
It is only applicable to molten polymers.

NOTE These methods are not suitable if the molecular structure of the polymer is modified during the test.