Plastics. Differential scanning calorimetry (DSC) - Determination of specific heat capacity

Plastics. Differential scanning calorimetry (DSC) - Determination of specific heat capacity

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1   Scope

This part of ISO 11357 specifies methods for determining the specific heat capacity of plastics by differential scanning calorimetry.