Plastics. Differential scanning calorimetry (DSC) - Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)

Plastics. Differential scanning calorimetry (DSC) - Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)

Regular price
£232.00
Sale price
£232.00
Regular price
£116.00
Sold out
Unit price
per 

1   Scope

This part of ISO 11357 specifies methods for the determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) of polymeric materials by means of differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized or compounded form, either as raw materials or finished products. It may be applicable to other plastics.