Plastics. Differential scanning calorimetry (DSC) - Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Plastics. Differential scanning calorimetry (DSC) - Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1   Scope

This part of ISO 11357 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.