Methods of test for footwear and footwear materials. Adhesives - Resistance of adhesive joints to heat (creep test)

Methods of test for footwear and footwear materials. Adhesives - Resistance of adhesive joints to heat (creep test)

Regular price
£142.00
Sale price
£142.00
Regular price
£71.00
Sold out
Unit price
per 

This Section of BS 5131 describes a laboratory test method for measuring the heat resistance of a bonded joint.

The main purpose of the method is to compare adhesives and as a consequence recommendations are given as to appropriate adherends.