Corrosion of metals and alloys. Stress corrosion testing - General guidance on testing procedures

Corrosion of metals and alloys. Stress corrosion testing - General guidance on testing procedures

Regular price
£232.00
Sale price
£232.00
Regular price
£116.00
Sold out
Unit price
per 

1   Scope

This part of ISO 7539 describes the general considerations that apply when designing and conducting tests to assess susceptibility of metals to stress corrosion.