Corrosion of metals and alloys. Guidelines for the evaluation of pitting corrosion
Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
SaleSold out
Unit price
/per
Adding product to your cart
1 Scope
This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.