Atomic layer deposition. Chemical characteristics and related process specifications of atomic layer deposition precursors

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1 Scope

This document defines the chemical characteristics and related process specifications of atomic layer deposition precursors, including assay content, metal purity and anion content specification.