What is BS EN 6041-Analysis of non-metallic materials by Differential Scanning Calorimetry about?
BS EN 6041 is a standard that serves technical specifications for analysis of non-metallic materials by Differential Scanning Calorimetry method that enables derivation of cure cycle and ageing behavior.
BS EN 6041 test method defines the procedure for determining the curing-characteristic and glass transition temperature of non-metallic materials (e.g. preimpregnated and neat resin systems, adhesives) for aerospace use by Differential Scanning Calorimetry (DSC).
The results obtained in BS EN 6041 can be useful for:
- Derivation of the optimum cure cycle
- Assessment of the condition of the resin
- Assessment of the ageing behavior of the resin
Note: BS EN 6041 does not give any directions to meet the health and safety requirements.
Who is BS EN 6041-Analysis of non-metallic materials by Differential Scanning Calorimetry for?
BS EN 6041 on analysis of non-metallic materials by Differential Scanning Calorimetry applies to:
- Manufacturers of adhesives and resins for aerospace applications
- Dealers and importers of adhesives and resins for aerospace applications
- Testing houses and labs in the aerospace industry
- Quality assurance services
Why should you use BS EN 6041-Analysis of non-metallic materials by Differential Scanning Calorimetry?
Curing in adhesives and resins is a chemical reaction to go from liquid (or thermoplastic) to solid. The glass transition temperature is the temperature at which cured adhesives and resins convert from rigidity to a glassy and rubber-like state. Both adhesives and resins are used in the aerospace industry, and assessing their condition is required to ensure optimal bonding strength.
BS EN 6041 provides you guidance on the Differential Scanning Calorimetry (DSC) method for analysis of non-metallic materials. BS EN 6041 also provides you with a step-by-step procedure for the method that enables you to do the method correctly and get accurate results.
BS EN 6041 also provides you guidance on conditioning which includes conditioning of material stored at ambient temperature, conditioning of material stored below ambient temperature, standard atmosphere for testing, the time interval between conditioning and testing that allows you to test for variable conditions and analyse results.
Guidance in BS EN 6041 enables you to analyse non-metallic materials such as resins and adhesives to assess their condition and ageing behavior.